Mold processing refers to the processing of forming and blank making tools. In addition, it also includes shear molds and die cutting molds. Sometimes defects occur during mold processing. Here are some ways to reduce mold processing defects.

First of all, use the cooling lubricant reasonably, play the three roles of cooling, washing and lubrication, keep the cooling, lubrication and cleaning, so as to control the grinding heat within the allowable range, and prevent the thermal deformation of the workpiece. Improve the cooling conditions during grinding, such as using oil immersed grinding wheel or internally cooled grinding wheel. When the cutting fluid is introduced into the center of the grinding wheel, the cutting fluid can directly enter the grinding area to play an effective cooling role and prevent the workpiece surface from burning.

mould

The second is to reasonably select the grinding parameters and adopt the precision grinding method with small radial feed or even fine grinding. If the radial feed and wheel speed are properly reduced, and the axial feed is increased, the contact area between the wheel and the workpiece will be reduced, and the heat dissipation condition will be improved, thus effectively controlling the increase of surface temperature.

Third: Reasonably select and trim the grinding wheel. The white corundum grinding wheel is better. Its performance is hard and brittle, and it is easy to generate new cutting edges. Therefore, the cutting force is small and the grinding heat is small. The medium grain size is used in the grain size, such as 46~60 mesh. The medium soft and soft (ZR1, ZR2 and R1, R2) are used in the hardness of the grinding wheel, that is, the coarse grain and low hardness grinding wheels. Good self excitation can reduce the cutting heat.


Send Inquiry